4.Lay
Fabric
The wet fabric is then applied to the surface with
our specially
design roll laminator, which has a built in tension
controller. |
 |
5.Wet
out Fabric
To assure the fabric is completely saturated with
epoxy, a roller is used to apply additional epoxy
where needed . |
 |
6.Eliminate
Air Voids
Fabric is pressed to the surface and air voids and
excess epoxy are removed . |
 |
7.Cure
Time
Let the Wellington cure for 7 days at ambient temperature
for maximum
performance.
|
 |
8.Top
Coat
Wellington can be top-coated in a variety of colors
for maintenance free protection and to match existing
structure.
|
|
|
|